F10092
Classification
| Country | Section | Category |
|---|---|---|
| USA | Iron, including Ductile Irons and Cast Irons | Cast Iron, Gray |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Ni, % | Ce, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| UNS | 90.985–93.36 | 3.25–3.75 | 0.04–0.1 | 0.1–0.4 | < 0.5 | < 0.2 | < 0.05 | 3.25–4 | < 0.015 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ni | % | Nickel |
| Ce | % | Cerium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |