F20000
Classification
| Country | Section | Category |
|---|---|---|
| USA | Iron, including Ductile Irons and Cast Irons | Cast Iron, Malleable |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | P, % | C, % |
|---|---|---|---|---|---|---|
| UNS | 93.6–96.71 | 0.9–1.9 | 0.15–1.25 | 0.02–0.2 | 0.02–0.15 | 2.2–2.9 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| P | % | Phosphorus |
| C | % | Carbon |