F41003
Classification
| Country | Section | Category |
|---|---|---|
| USA | Iron, including Ductile Irons and Cast Irons | Cast Iron, Gray, Austenitic |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % |
|---|---|---|---|---|---|---|---|---|
| UNS | 64.08–77.5 | 1–2.8 | 0.5–1.5 | 3–6 | < 0.5 | 18–22 | < 0.12 | < 3 |