F43030
Classification
| Country |
Section |
Category |
| USA |
Iron, including Ductile Irons and Cast Irons |
Cast Iron, Ductile (Nodular), Austenitic |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| UNS |
66.5–73.6 |
2–3 |
1.9–2.5 |
< 0.5 |
20–24 |
< 0.15 |
2.5–3 |
< 0.05 |
< 0.3 |