J02505
Classification
| Country | Section | Category |
|---|---|---|
| USA | Cast Steels (except tool steels) | Carbon Steel Casting |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|
| UNS | > 97.865 | < 0.6 | < 1.2 | < 0.04 | < 0.25 | < 0.045 |
Information on suppliers
Analogues
| CIS, Russia, Ukraine |
|---|
| 20GL |
Standards
| Standard | Description |
|---|---|
| UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |