J12047
Classification
| Country | Section | Category |
|---|---|---|
| USA | Cast Steels (except tool steels) | Alloy Steel Casting |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|
| UNS | 96.4–98.05 | 0.2–0.8 | 0.65–0.95 | 0.4–0.6 | 0.4–0.7 | < 0.025 | 0.15–0.25 | < 0.025 | 0.15–0.25 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |