J12582
Classification
| Country | Section | Category |
|---|---|---|
| USA | Cast Steels (except tool steels) | Alloy Steel Casting |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | V, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| UNS | 94.97–98.5 | < 0.6 | < 1.2 | < 0.4 | < 0.5 | 1.5–2 | < 0.03 | < 0.025 | < 0.25 | < 0.025 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| V | % | Vanadium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |