J91109
Classification
| Country | Section | Category |
|---|---|---|
| USA | Cast Steels (except tool steels) | Austenitic Manganese Steel Casting, Alloy Steel Casting |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | P, % | C, % |
|---|---|---|---|---|---|
| UNS | 86.58–98.95 | < 1 | < 11 | < 0.07 | 1.05–1.35 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| P | % | Phosphorus |
| C | % | Carbon |