J91422
Classification
| Country |
Section |
Category |
| USA |
Cast Steels (except tool steels) |
Austenitic Manganese Steel Casting, Alloy Steel Casting |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| UNS |
81.36–85.8 |
< 1 |
0.5–1 |
11–12.5 |
0.5–1 |
0.2–0.3 |
< 0.03 |
0.2–0.28 |
< 0.03 |
0.9–1.25 |
0.9–1.25 |