Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Nb, % |
N, % |
| UNS |
69.82–74.8 |
0.5–1 |
< 0.7 |
15.5–16.7 |
2.8–3.5 |
3.6–4.6 |
< 0.04 |
< 0.06 |
< 0.03 |
2.8–3.5 |
< 0.05 |