J92240
Classification
| Country |
Section |
Category |
| USA |
Cast Steels (except tool steels) |
Alloy Steel Casting Precipitation Hardening, Cast Cr-Ni-Mo Stainless Steel, Cr-Ni, Cr-Mn-Ni-Si-N |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
| UNS |
72.45–77.25 |
0.5–1 |
< 0.7 |
13.5–14.7 |
3–3.5 |
3.75–4.75 |
< 0.02 |
< 0.06 |
< 0.02 |
2–2.75 |
< 0.05 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |