J92511
Classification
| Country |
Section |
Category |
| USA |
Cast Steels (except tool steels) |
Alloy Steel Casting Precipitation Hardening, Cast Cr-Ni-Mo Stainless Steel, Cr-Ni, Cr-Mn-Ni-Si-N |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| UNS |
65.08–74.7 |
< 1 |
< 2 |
17–20 |
< 0.5 |
8–10 |
0.15–0.35 |
< 0.12 |
0.15–0.35 |
< 0.6 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |