J92805
Classification
| Country |
Section |
Category |
| USA |
Cast Steels (except tool steels) |
Alloy Steel Casting Precipitation Hardening, Cast Cr-Ni-Mo Stainless Steel, Cr-Ni, Cr-Mn-Ni-Si-N |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
| UNS |
59.04–68.8 |
< 1.5 |
< 1.5 |
23–26 |
8–11 |
< 0.04 |
< 0.08 |
< 0.04 |
< 0.5 |
0.2–0.3 |