J93150
Classification
| Country |
Section |
Category |
| USA |
Cast Steels (except tool steels) |
Stainless Steel Casting, Cr-Ni-Mo Stainless Steel, Alloy Steel, Maraging Ferritic-Austenic, Duplex, Alloy Steel Casting |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Co, % |
Ti, % |
Ni, % |
Al, % |
P, % |
C, % |
S, % |
Mo, % |
| UNS |
64.7–68.4 |
< 0.1 |
< 0.1 |
8.5–9.5 |
0.55–0.85 |
18–19 |
0.05–0.2 |
< 0.01 |
< 0.03 |
< 0.01 |
4.5–5.5 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |