J93404
Classification
| Country |
Section |
Category |
| USA |
Cast Steels (except tool steels) |
Stainless Steel Casting, Cr-Ni-Mo Stainless Steel, Alloy Steel, Maraging Ferritic-Austenic, Duplex, Alloy Steel Casting |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
C, % |
Mo, % |
N, % |
| UNS |
58.17–65.9 |
< 1 |
< 1.5 |
24–26 |
6–8 |
< 0.03 |
4–5 |
0.1–0.3 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| C |
% |
Carbon |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |