J94651
Classification
| Country |
Section |
Category |
| USA |
Cast Steels (except tool steels) |
Stainless Steel Casting, Cr-Ni-Mo Stainless Steel, Alloy Steel, Maraging Ferritic-Austenic, Duplex, Alloy Steel Casting |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
| UNS |
41.41–50.32 |
< 1 |
< 2 |
20–22 |
< 0.75 |
23.5–25.5 |
< 0.04 |
< 0.03 |
< 0.01 |
6–7 |
0.18–0.26 |