K02011
Classification
| Country |
Section |
Category |
| USA |
Miscellaneous steels and ferrous alloys, including Maraging, Stainless Steel, HSLA, Iron-Base Superalloys |
Carbon Steel, Carbon Steel with Special Magnetic Properties, Steel Welding Rod, Enameling Steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
V, % |
Al, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
| UNS |
97.07–98.75 |
0.1–0.35 |
1.15–1.5 |
< 0.15 |
< 0.15 |
< 0.25 |
< 0.12 |
< 0.06 |
< 0.035 |
< 0.2 |
< 0.015 |
< 0.05 |
< 0.05 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |