K02306
Classification
| Country |
Section |
Category |
| USA |
Miscellaneous steels and ferrous alloys, including Maraging, Stainless Steel, HSLA, Iron-Base Superalloys |
Carbon Steel, Carbon Steel with Special Magnetic Properties, Steel Welding Rod, Enameling Steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cu, % |
P, % |
C, % |
S, % |
N, % |
| UNS |
> 97.715 |
< 0.4 |
< 1.35 |
< 0.2 |
< 0.04 |
< 0.23 |
< 0.05 |
< 0.015 |