K03810
Classification
| Country |
Section |
Category |
| USA |
Miscellaneous steels and ferrous alloys, including Maraging, Stainless Steel, HSLA, Iron-Base Superalloys |
Carbon Steel, Carbon Steel with Special Magnetic Properties, Steel Welding Rod, Enameling Steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| UNS |
96.715–98.1395 |
0.15–0.35 |
0.0005–0.005 |
0.75–1 |
0.3–0.55 |
< 0.35 |
0.2–0.4 |
< 0.025 |
0.38–0.43 |
< 0.025 |
0.08–0.15 |