K31116
Classification
| Country |
Section |
Category |
| USA |
Miscellaneous steels and ferrous alloys, including Maraging, Stainless Steel, HSLA, Iron-Base Superalloys |
Alloy Steel, Alloy Steel Electrode and Welding Wire, High-Strength Low-Alloy Steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Mn, % |
Cr, % |
Cu, % |
Sb, % |
As, % |
P, % |
C, % |
S, % |
Mo, % |
| UNS |
94.16–96.35 |
0.05–0.3 |
< 0.01 |
0.4–0.8 |
2.25–3.3 |
< 0.15 |
< 0.005 |
< 0.005 |
< 0.01 |
0.05–0.15 |
< 0.01 |
0.9–1.1 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Sb |
% |
Antimony |
| As |
% |
Arsenic |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |