K31835
Classification
| Country |
Section |
Category |
| USA |
Miscellaneous steels and ferrous alloys, including Maraging, Stainless Steel, HSLA, Iron-Base Superalloys |
Alloy Steel, Alloy Steel Electrode and Welding Wire, High-Strength Low-Alloy Steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Ca, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
Se, % |
| UNS |
94.588–96.44 |
< 0.1 |
< 0.002 |
< 0.015 |
0.3–0.6 |
2–2.5 |
< 0.03 |
< 0.2 |
< 0.25 |
0.25–0.35 |
< 0.015 |
0.11–0.15 |
< 0.01 |
< 0.07 |
0.9–1.1 |
< 0.02 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Ca |
% |
Calcium |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |
| Se |
% |
Selenium |