K32045
Classification
| Country |
Section |
Category |
| USA |
Miscellaneous steels and ferrous alloys, including Maraging, Stainless Steel, HSLA, Iron-Base Superalloys |
Alloy Steel, Alloy Steel Electrode and Welding Wire, High-Strength Low-Alloy Steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
| UNS |
93.052–96.3 |
0.15–0.35 |
0.1–0.4 |
1–1.8 |
< 0.02 |
< 0.025 |
2.25–3.5 |
< 0.03 |
< 0.015 |
< 0.2 |
< 0.008 |
0.2–0.6 |