K91271
Classification
| Country |
Section |
Category |
| USA |
Miscellaneous steels and ferrous alloys, including Maraging, Stainless Steel, HSLA, Iron-Base Superalloys |
Alloy Steel, Superstrength, Ferritic Cr-Mo-V, Mg, Nonmagnetic, Ni-Co, Electrical Heating, Martensitic, Fe-Co Alloy, Nickel Steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
N, % |
W, % |
| UNS |
81.325–87.6495 |
< 0.5 |
0.0005–0.005 |
< 0.7 |
10–12.5 |
0.3–0.7 |
< 0.5 |
0.15–0.3 |
< 0.02 |
0.07–0.14 |
< 0.01 |
0.04–0.1 |
0.25–0.6 |
0.04–0.1 |
1.5–2.5 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |
| W |
% |
Tungsten |