Main
-
Brand
-
USA
-
K00001 - K99999 (Miscellaneous steels and ferrous alloys, including Maraging, Stainless Steel, HSLA, Iron-Base Superalloys)
-
K90901 - K95000 (Alloy Steel, Superstrength, Ferritic Cr-Mo-V, Mg, Nonmagnetic, Ni-Co, Electrical Heating, Martensitic, Fe-Co Alloy, Nickel Steel)
Classification
| Country |
Section |
Category |
| USA |
Miscellaneous steels and ferrous alloys, including Maraging, Stainless Steel, HSLA, Iron-Base Superalloys |
Alloy Steel, Superstrength, Ferritic Cr-Mo-V, Mg, Nonmagnetic, Ni-Co, Electrical Heating, Martensitic, Fe-Co Alloy, Nickel Steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
V, % |
C, % |
Mo, % |
W, % |
| UNS |
77.5–86.3 |
< 0.5 |
< 0.5 |
3–5 |
1–2.5 |
0.7–1 |
4–6 |
5–7 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| V |
% |
Vanadium |
| C |
% |
Carbon |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |