K91955
Classification
| Country |
Section |
Category |
| USA |
Miscellaneous steels and ferrous alloys, including Maraging, Stainless Steel, HSLA, Iron-Base Superalloys |
Alloy Steel, Superstrength, Ferritic Cr-Mo-V, Mg, Nonmagnetic, Ni-Co, Electrical Heating, Martensitic, Fe-Co Alloy, Nickel Steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
| UNS |
70.645–79.9 |
0.2–0.65 |
16–20 |
3.5–6 |
< 2 |
< 0.08 |
0.4–0.6 |
< 0.025 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |