N03220
Classification
| Country | Section | Category |
|---|---|---|
| USA | Nickel and Nickel Alloys | Nickel and Nickel Alloys |
Chemical composition
| Standard | Fe, % | Mg, % | Cu, % | Ni, % | Al, % | C, % | O, % | N, % |
|---|---|---|---|---|---|---|---|---|
| UNS | < 0.015 | < 0.001 | < 0.02 | 99.437–99.7 | < 0.001 | 0.3–0.5 | < 0.025 | < 0.001 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Mg | % | Magnesium |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| C | % | Carbon |
| O | % | Oxygen |
| N | % | Nitrogen |