N06009
Classification
| Country | Section | Category |
|---|---|---|
| USA | Nickel and Nickel Alloys | Nickel and Nickel Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | C, % | S, % | Nb, % |
|---|---|---|---|---|---|---|---|---|
| UNS | < 1 | 0.75–1.6 | < 2.5 | 19–21 | 72.24–79.5 | < 0.15 | < 0.01 | 0.75–1.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |