N06075
Classification
| Country | Section | Category |
|---|---|---|
| USA | Nickel and Nickel Alloys | Nickel and Nickel Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | Al, % | Pb, % | C, % |
|---|---|---|---|---|---|---|---|---|---|---|
| UNS | < 2 | < 1 | < 1 | 18–21 | 0.15–0.5 | < 0.5 | 73.44–81.77 | < 0.4 | < 0.01 | 0.08–0.15 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |
| C | % | Carbon |