N06255
Classification
| Country |
Section |
Category |
| USA |
Nickel and Nickel Alloys |
Nickel and Nickel Alloys |
Chemical composition
| Standard |
Si, % |
Sn, % |
Mn, % |
Co, % |
Cr, % |
Cu, % |
Ni, % |
Pb, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| UNS |
< 1 |
< 0.025 |
< 1 |
2.5–4 |
23–26 |
< 0.5 |
47–52 |
< 0.025 |
< 0.03 |
< 0.03 |
< 0.03 |
6–9 |
2.5–4 |