N06804
Classification
| Country | Section | Category |
|---|---|---|
| USA | Nickel and Nickel Alloys | Nickel and Nickel Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Ni, % | C, % | S, % | W, % |
|---|---|---|---|---|---|---|---|---|---|
| UNS | 17–20 | < 0.75 | < 1.5 | < 5 | 28–31 | 39–43 | < 0.1 | < 0.015 | 1–2 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ni | % | Nickel |
| C | % | Carbon |
| S | % | Sulfur |
| W | % | Tungsten |