N07090
Classification
| Country | Section | Category |
|---|---|---|
| USA | Nickel and Nickel Alloys | Nickel and Nickel Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | C, % |
|---|---|---|---|---|---|---|---|---|
| UNS | < 8 | < 1.5 | < 1 | 18–21 | 2.5–3.5 | < 0.5 | 64.37–79.5 | < 0.13 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| UNS |