N07520
Classification
| Country |
Section |
Category |
| USA |
Nickel and Nickel Alloys |
Nickel and Nickel Alloys |
Chemical composition
| Standard |
Fe, % |
Co, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
Al, % |
C, % |
Nb, % |
Mo, % |
N, % |
| UNS |
< 6 |
< 1 |
18–20 |
< 0.6 |
< 0.5 |
58.49–72.1 |
0.4–0.8 |
< 0.06 |
4.5–5.5 |
5–7 |
< 0.05 |