N08332
Classification
| Country |
Section |
Category |
| USA |
Nickel and Nickel Alloys |
Nickel and Nickel Alloys |
Chemical composition
| Standard |
Si, % |
Sn, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
Al, % |
Pb, % |
P, % |
C, % |
S, % |
Mo, % |
| UNS |
0.75–1.5 |
< 0.025 |
< 2 |
17–20 |
0.2–0.6 |
< 1 |
34–37 |
0.1–0.5 |
< 0.005 |
< 0.03 |
0.05–0.1 |
< 0.03 |
< 0.75 |