N08421
Classification
| Country | Section | Category |
|---|---|---|
| USA | Nickel and Nickel Alloys | Nickel and Nickel Alloys |
Chemical composition
| Standard | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | Al, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|
| UNS | < 0.5 | < 1 | 20–22 | 0.6–1 | 1.5–2 | 39–41 | < 0.2 | < 0.025 | < 0.03 | < 0.7 |