N08802
Classification
| Country | Section | Category |
|---|---|---|
| USA | Nickel and Nickel Alloys | Nickel and Nickel Alloys |
Chemical composition
| Standard | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | Al, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| UNS | < 0.75 | < 1.5 | 19–23 | 0.25–1.25 | < 0.75 | 30–35 | 0.15–1 | 0.2–0.5 | < 0.015 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| C | % | Carbon |
| S | % | Sulfur |