N10675
Classification
| Country |
Section |
Category |
| USA |
Nickel and Nickel Alloys |
Nickel and Nickel Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Co, % |
Cr, % |
Ti, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
W, % |
| UNS |
< 3.5 |
< 0.1 |
< 3 |
27–33 |
1–3 |
0.2–0.8 |
< 65 |
< 0.2 |
< 0.03 |
< 0.01 |
< 0.01 |
< 1 |
26–30 |
< 1 |