N12160
Classification
| Country |
Section |
Category |
| USA |
Nickel and Nickel Alloys |
Nickel and Nickel Alloys |
Chemical composition
| Standard |
Si, % |
B, % |
Bi, % |
Mn, % |
Co, % |
Cr, % |
Ni, % |
Al, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
| UNS |
2.4–3 |
0.01–0.02 |
< 5.0E-5 |
< 1.5 |
9–11 |
26–30 |
15.78495–30.09 |
4.75–5.25 |
< 0.03 |
< 0.15 |
< 0.015 |
0.75–1.25 |
17.69495–41.30505 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Bi |
% |
Bismuth |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |