N26455
Classification
| Country | Section | Category |
|---|---|---|
| USA | Nickel and Nickel Alloys | Nickel and Nickel Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % | Nb, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|
| UNS | < 5 | < 0.8 | < 1 | 15–17.5 | 53.62–66.85 | < 0.03 | < 0.02 | < 0.03 | 3.15–4.5 | 15–17.5 |