R20600
Classification
| Country | Section | Category |
|---|---|---|
| USA | Reactive and Refractory Metals and Alloys | Chromium |
Chemical composition
| Standard | Si, % | Mn, % | Cr, % | P, % | S, % | Hf, % |
|---|---|---|---|---|---|---|
| UNS | < 1 | < 0.3 | 56.66–63.34 | < 0.02 | < 0.02 | 36.66–42 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| P | % | Phosphorus |
| S | % | Sulfur |
| Hf | % | Hafnium |