R30003
Classification
| Country | Section | Category |
|---|---|---|
| USA | Reactive and Refractory Metals and Alloys | Cobalt |
Chemical composition
| Standard | Be, % | Mn, % | Co, % | Cr, % | Ni, % | C, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|
| UNS | < 0.06 | 1.5–2.5 | 41–44 | 19–21 | 15–16 | < 0.15 | 6–8 | 2.3–3.3 |
Information on suppliers
Analogues
| Germany |
|---|
| 2.4711 (CoCr20Ni15Mo) |
Standards
| Standard | Description |
|---|---|
| UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Be | % | Beryllium |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ni | % | Nickel |
| C | % | Carbon |
| Mo | % | Molybdenum |
| W | % | Tungsten |