Main
-
Brand
-
USA
-
S00001 - S99999 (Stainless Steels, including Precipitation Hardening Stainless Steel and Iron-Based Superalloys)
-
S20100 - S39000 (Austenitic Cr-Mn-Ni-(Si, Mo, Cu, Al) Stainless Steel, Cr-Mn-Ni, Cr-Ni Heat Resisting Steel, Hardenable Cr-Ni-(Si, Ti, Mo, Al))
S21500
Classification
| Country |
Section |
Category |
| USA |
Stainless Steels, including Precipitation Hardening Stainless Steel and Iron-Based Superalloys |
Austenitic Cr-Mn-Ni-(Si, Mo, Cu, Al) Stainless Steel, Cr-Mn-Ni, Cr-Ni Heat Resisting Steel, Hardenable Cr-Ni-(Si, Ti, Mo, Al) |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
Cr, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
| UNS |
61.721–69.537 |
0.2–1.2 |
0.003–0.009 |
5.5–7 |
14–16 |
9–11 |
0.15–0.4 |
< 0.04 |
0.06–0.15 |
< 0.03 |
0.75–1.25 |
0.8–1.2 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |