S30433
Classification
| Country |
Section |
Category |
| USA |
Stainless Steels, including Precipitation Hardening Stainless Steel and Iron-Based Superalloys |
Austenitic Cr-Mn-Ni-(Si, Mo, Cu, Al) Stainless Steel, Cr-Mn-Ni, Cr-Ni Heat Resisting Steel, Hardenable Cr-Ni-(Si, Ti, Mo, Al) |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
Al, % |
P, % |
C, % |
S, % |
Nb, % |
N, % |
| UNS |
63.662–72.246 |
< 1 |
0.001–0.01 |
< 2 |
17–19 |
2.5–3.5 |
8–10 |
0.003–0.03 |
< 0.045 |
< 0.003 |
< 0.03 |
0.2–0.6 |
0.05–0.12 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| N |
% |
Nitrogen |