S31260
Classification
| Country |
Section |
Category |
| USA |
Stainless Steels, including Precipitation Hardening Stainless Steel and Iron-Based Superalloys |
Austenitic Cr-Mn-Ni-(Si, Mo, Cu, Al) Stainless Steel, Cr-Mn-Ni, Cr-Ni Heat Resisting Steel, Hardenable Cr-Ni-(Si, Ti, Mo, Al) |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
W, % |
| UNS |
59.56–67.6 |
< 0.75 |
< 1 |
24–26 |
0.2–0.8 |
5.5–7.5 |
< 0.03 |
< 0.03 |
< 0.03 |
2.5–3.5 |
0.1–0.3 |
0.1–0.5 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |
| W |
% |
Tungsten |