S41428
Classification
| Country |
Section |
Category |
| USA |
Stainless Steels, including Precipitation Hardening Stainless Steel and Iron-Based Superalloys |
Martensitic Cr, Cr-Ni-Mo Stainless Steel, Ferritic Cr with Ti, Ni, Mo, Hardenable |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
| UNS |
79.985–84 |
< 0.35 |
0.65–1.05 |
11.25–12.75 |
< 0.01 |
2.25–3.25 |
0.25–0.4 |
< 0.02 |
0.1–0.17 |
< 0.015 |
1.5–2 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |