S50481
Classification
| Country |
Section |
Category |
| USA |
Stainless Steels, including Precipitation Hardening Stainless Steel and Iron-Based Superalloys |
Cr Heat Resisting Steels and Filler Metal |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
V, % |
Al, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
N, % |
| UNS |
86.648–90.8 |
0.05–0.5 |
0.3–0.65 |
8–10.5 |
< 0.1 |
< 0.05 |
< 0.04 |
< 0.012 |
< 0.1 |
< 0.03 |
0.02–0.1 |
0.8–1.2 |
0.03–0.07 |