TU 14-1-1589-76
Information about the standard
| Standard | TU 14-1-1589-76 |
|---|---|
| Country | CIS, Russia, Ukraine |
| Type of standard | ГОСТ ТУ |
| Materials | EI787-VD, HN35VTU-VD, HN35VTYU |
| Standard | TU 14-1-1589-76 |
|---|---|
| Country | CIS, Russia, Ukraine |
| Type of standard | ГОСТ ТУ |