TU 14-1-4481-88
Information about the standard
| Standard | TU 14-1-4481-88 |
|---|---|
| Country | CIS, Russia, Ukraine |
| Type of standard | ГОСТ ТУ |
| Materials | 10H15N27T3MR-VD, 10X16H27T3MR, EP700-VD |
| Standard | TU 14-1-4481-88 |
|---|---|
| Country | CIS, Russia, Ukraine |
| Type of standard | ГОСТ ТУ |
| Materials | 10H15N27T3MR-VD, 10X16H27T3MR, EP700-VD |