1.0036 (S235JRG1)
For thicknesses up to 25 mm.
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Steels | Base Steels |
Chemical composition
| Standard | Fe, % | Mn, % | P, % | C, % | S, % | N, % |
|---|---|---|---|---|---|---|
| EN 10025 | > 98.333 | < 1.4 | < 0.045 | < 0.17 | < 0.045 | < 0.007 |
Information on suppliers
Properties
| Property |
|---|
| Density: 7.86 g / cm3 |
Analogues
| CIS, Russia, Ukraine | Germany | USA |
|---|---|---|
| 18kp | USt 37-2 G | S235JR |
Standards
| Standard | Description |
|---|---|
| EN 10025 | |
| DIN 1623 Part 2 | |
| DIN EN 10025:1990 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Mn | % | Manganese |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| N | % | Nitrogen |