18kp
for welded constructions in the form of sheets of different thicknesses and shaped profiles.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Carbonaceous quality structural steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | As, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1050-88 | 98.435–99.58 | < 0.06 | 0.3–0.5 | < 0.15 | < 0.2 | < 0.3 | < 0.08 | < 0.035 | 0.12–0.2 | < 0.04 |
Information on suppliers
Mechanical properties at 20 °C
Analogues
| USA | Germany |
|---|---|
| K02502 | 1.0036 (S235JRG1) |
Standards
| Standard | Description |
|---|---|
| GOST 1050-88 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| As | % | Arsenic |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |