1.0314 (C2C)

Classification

Country Section Category
Germany Non-alloy Steels Steels with Average C < 0,12% or Rm < 400 MPa

Chemical composition

Standard Fe, % Si, % Mn, % Al, % P, % C, % S, %
EN 10263-2 99.365–99.78 < 0.1 0.2–0.4 0.02–0.06 < 0.02 < 0.03 < 0.025

Information on suppliers

Mechanical properties at 20 °C

Rolling Standard Size, mm Tension Classifiers $$\sigma _{U}$$, $$MPa$$ $$\psi$$, % Treatment
300–450 68–80

Свойства

Свойство
Плотность: 7.87 г/см3

Analogues

Germany CIS, Russia, Ukraine USA
QSt 32-3 05kp 1005 AISI

Standards

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Mn % Manganese
Al % Aluminium
P % Phosphorus
C % Carbon
S % Sulfur

Description of mechanical properties

Parameter Units of measurement Description
$$\sigma _{U}$$ $$MPa$$ Ultimate tensile strength
$$\psi$$ % Reduction in cross section on fracture